Poley, L., Blue, A., Bloch, I., Buttar, C., Fadeyev, V., Fernandez-Tejero, J., et al. (2019). Mapping the depleted area of silicon diodes using a micro-focused X-ray beam. J. Instrum., 14, P03024–14pp.
Abstract: For the Phase-II Upgrade of the ATLAS detector at CERN, the current ATLAS Inner Detector will be replaced with the ATLAS Inner Tracker (ITk). The ITk will be an all-silicon detector, consisting of a pixel tracker and a strip tracker. Sensors for the ITk strip tracker are required to have a low leakage current up to bias voltages of 500V to maintain a low noise and power dissipation. In order to minimise sensor leakage currents, particularly in the high-radiation environment inside the ATLAS detector, sensors are foreseen to be operated at low temperatures and to be manufactured from wafers with a high bulk resistivity of several k Omega.cm. Simulations showed the electric field inside sensors with high bulk resistivity to extend towards the sensor edge, which could lead to increased surface currents for narrow dicing edges. In order to map the electric field inside biased silicon sensors with high bulk resistivity, three diodes from ATLAS silicon strip sensor prototype wafers were studied with a monochromatic, micro-focused X-ray beam at the Diamond Light Source (Didcot, U.K.). For all devices under investigation, the electric field inside the diode was mapped and its dependence on the applied bias voltage was studied.
|
ATLAS Collaboration(Aad, G. et al), Amos, K. R., Aparisi Pozo, J. A., Bailey, A. J., Cabrera Urban, S., Cardillo, F., et al. (2022). Operation and performance of the ATLAS semiconductor tracker in LHC Run 2. J. Instrum., 17(1), P01013–56pp.
Abstract: The semiconductor tracker (SCT) is one of the tracking systems for charged particles in the ATLAS detector. It consists of 4088 silicon strip sensor modules. During Run 2 (2015-2018) the Large Hadron Collider delivered an integrated luminosity of 156 fb(-1) to the ATLAS experiment at a centre-of-mass proton-proton collision energy of 13 TeV. The instantaneous luminosity and pile-up conditions were far in excess of those assumed in the original design of the SCT detector. Due to improvements to the data acquisition system, the SCT operated stably throughout Run 2. It was available for 99.9% of the integrated luminosity and achieved a data-quality efficiency of 99.85%. Detailed studies have been made of the leakage current in SCT modules and the evolution of the full depletion voltage, which are used to study the impact of radiation damage to the modules. '
|
Mandic, I., Cindro, V., Debevc, J., Gorisek, A., Hiti, B., Kramberger, G., et al. (2022). Study of neutron irradiation effects in Depleted CMOS detector structures. J. Instrum., 17(3), P03030–13pp.
Abstract: In this paper the results of Edge-TCT and I-V measurements with passive test structures made in LFoundry 150 nm HV-CMOS process on p-type substrates with different initial resistivities ranging from 0.5 to 3 k Omega cm are presented. Samples were irradiated with reactor neutrons up to a fluence of 2.10(15) n(eq)/cm(2). The depletion depth was measured with Edge-TCT. The effective space charge concentration N-eff was estimated from the dependence of the depletion depth on bias voltage and studied as a function of neutron fluence. The dependence of N-eff on fluence changes with initial acceptor concentration in agreement with other measurements with p-type silicon. A long term accelerated annealing study of N-eff and detector current up to 1280 minutes at 60 degrees C was made. It was found that N-eff and current in reverse biased detector behave as expected for irradiated silicon.
|
Unno, Y. et al, Bernabeu, J., Lacasta, C., Solaz, C., & Soldevila, U. (2023). Specifications and pre-production of n plus -in-p large-format strip sensors fabricated in 6-inch silicon wafers, ATLAS18, for the Inner Tracker of the ATLAS Detector for High-Luminosity Large Hadron Collider. J. Instrum., 18(3), T03008–29pp.
Abstract: The ATLAS experiment is constructing new all-silicon inner tracking system for HL-LHC. The strip detectors cover the radial extent of 40 to 100 cm. A new approach is adopted to use p-type silicon material, making the readout in n+-strips, so-called n+-in-p sensors. This allows for enhanced radiation tolerance against an order of magnitude higher particle fluence compared to the LHC. To cope with varying hit rates and occupancies as a function of radial distance, there are two barrel sensor types, the short strips (SS) for the inner 2 and the long strips (LS) for the outer 2 barrel cylinders, respectively. The barrel sensors exhibit a square, 9.8 x 9.8 cm2, geometry, the largest possible sensor area from a 6-inch wafer. The strips are laid out in parallel with a strip pitch of 75.5 μm and 4 or 2 rows of strip segments. The strips are AC-coupled and biased via polysilicon resistors. The endcap sensors employ a “stereo-annulus” geometry exhibiting a skewed-trapezoid shapes with circular edges. They are designed in 6 unique shapes, R0 to R5, corresponding to progressively increasing radial extents and which allows them to fit within the petal geometry and the 6-inch wafer maximally. The strips are in fan-out geometry with an in-built rotation angle, with a mean pitch of approximately 75 μm and 4 or 2 rows of strip segments. The eight sensor types are labeled as ATLAS18xx where xx stands for SS, LS, and R0 to R5. According to the mechanical and electrical specifications, CAD files for wafer processing were laid out, following the successful designs of prototype barrel and endcap sensors, together with a number of optimizations. A pre-production was carried out prior to the full production of the wafers. The quality of the sensors is reviewed and judged excellent through the test results carried out by vendor. These sensors are used for establishing acceptance procedures and to evaluate their performance in the ATLAS collaboration, and subsequently for pre-production of strip modules and stave and petal structures.
|