Latonova, V. et al, Bernabeu, J., Lacasta, C., Solaz, C., & Soldevila, U. (2023). Characterization of the polysilicon resistor in silicon strip sensors for ATLAS inner tracker as a function of temperature, pre- and post-irradiation. Nucl. Instrum. Methods Phys. Res. A, 1050, 168119–5pp.
Abstract: The high luminosity upgrade of the Large Hadron Collider, foreseen for 2029, requires the replacement of the ATLAS Inner Detector with a new all-silicon Inner Tracker (ITk). The expected ultimate total integrated luminosity of 4000 fb(-1) means that the strip part of the ITk detector will be exposed to the total particle fluences and ionizing doses reaching the values of 1.6 center dot 10(15) MeVn(eq)/cm(2) and 0.66MGy, respectively, including a safety factor of 1.5. Radiation hard n(+)-in-p micro-strip sensors were developed by the ATLAS ITk strip collaboration and are produced by Hamamatsu Photonics K.K. The active area of each ITk strip sensor is delimited by the n-implant bias ring, which is connected to each individual n(+) implant strip by a polysilicon bias resistor. The total resistance of the polysilicon bias resistor should be within a specified range to keep all the strips at the same potential, prevent the signal discharge through the grounded bias ring and avoid the readout noise increase. While the polysilicon is a ubiquitous semiconductor material, the fluence and temperature dependence of its resistance is not easily predictable, especially for the tracking detector with the operational temperature significantly below the values typical for commercial microelectronics. Dependence of the resistance of polysilicon bias resistor on the temperature, as well as on the total delivered fluence and ionizing dose, was studied on the specially-designed test structures called ATLAS Testchips, both before and after their irradiation by protons, neutrons, and gammas to the maximal expected fluence and ionizing dose. The resistance has an atypical negative temperature dependence. It is different from silicon, which shows that the grain boundary has a significant contribution to the resistance. We discuss the contributions by parameterizing the activation energy of the polysilicon resistance as a function of the temperature for unirradiated and irradiated ATLAS Testchips.
|
|
|
Fernandez-Tejero, J., Bartl, U., Docke, M., Fadeyev, V., Fleta, C., Hacker, J., et al. (2020). Design and evaluation of large area strip sensor prototypes for the ATLAS Inner Tracker detector. Nucl. Instrum. Methods Phys. Res. A, 981, 164536–6pp.
Abstract: The ATLAS community is facing the last stages prior to the production of the upgraded silicon strip Inner Tracker for the High-Luminosity Large Hadron Collider. An extensive Market Survey was carried out in order to evaluate the capability of different foundries to fabricate large area silicon strip sensors, satisfying the ATLAS specifications. The semiconductor manufacturing company, Infineon Technologies AG, was one of the two foundries, along with Hamamatsu Photonics K.K., that reached the last stage of the evaluation for the production of the new devices. The full prototype wafer layout for the participation of Infineon, called ATLAS17LS-IFX, was designed using a newly developed Python-based Automatic Layout Generation Tool, able to rapidly design sensors with different characteristics and dimensions based on a few geometrical and technological input parameters. This work presents the layout design process and the results obtained from the evaluation of the new Infineon large area sensors before and after proton and neutron irradiations, up to fluences expected in the inner layers of the future ATLAS detector.
|
|
|
Hara, K. et al, Escobar, C., Garcia, C., Lacasta, C., Miñano, M., & Soldevila, U. (2020). Charge collection study with the ATLAS ITk prototype silicon strip sensors ATLAS17LS. Nucl. Instrum. Methods Phys. Res. A, 983, 164422–6pp.
Abstract: The inner tracker of the ATLAS detector is scheduled to be replaced by a completely new silicon-based inner tracker (ITk) for the Phase-II of the CERN LHC (HL-LHC). The silicon strip detector covers the volume 40 < R < 100 cm in the radial and vertical bar z vertical bar <300 cm in the longitudinal directions. The silicon sensors for the detector will be fabricated using the n(+)-on-p 6-inch wafer technology, for a total of 22,000 wafers. Intensive studies were carried out on the final prototype sensors ATLAS17LS fabricated by Hamamatsu Photonics (HPK). The charge collection properties were examined using penetrating Sr-90 beta-rays and the ALIBAVA fast readout system for the miniature sensors of 1 cm xl cm in area. The samples were irradiated by protons in the 27 MeV Birmingham Cyclotron, the 70 MeV CYRIC at Tohoku University, and the 24 GeV CERN-PS, and by neutrons at Ljubljana TAIGA reactor for fluence values up to 2 x 10(15) n(eq)/cm(2). The change in the charge collection with fluence was found to be similar to the previous prototype ATLAS12, and acceptable for the ITk. Sensors with two active thicknesses, 300 μm (standard) and 240 μm (thin), were compared and the difference in the charge collection was observed to be small for bias voltages up to 500 V. Some samples were also irradiated with gamma radiation up to 2 MGy, and the full depletion voltage was found to decrease with the dose. This was caused by the Compton electrons due to the( 60)Co gamma radiation. To summarize, the design of the ATLAS17LS and technology for its fabrication have been verified for implementation in the ITk. We are in the stage of sensor pre-production with the first sensors already delivered in January of 2020.
|
|
|
Fernandez-Tejero, J. et al, & Soldevila, U. (2020). Humidity sensitivity of large area silicon sensors: Study and implications. Nucl. Instrum. Methods Phys. Res. A, 978, 164406–6pp.
Abstract: The production of large area sensors is one of the main challenges that the ATLAS collaboration faces for the new Inner-Tracker full-silicon detector. During the prototype fabrication phase for the High Luminosity Large Hadron Collider upgrade, several ATLAS institutes observed indications of humidity sensitivity of large area sensors, even at relative humidities well below the dew point. Specifically, prototype Barrel and End-Cap silicon strip sensors fabricated in 6-inch wafers manifest a prompt decrease of the breakdown voltage when operating under high relative humidity, adversely affecting the performance of the sensors. In addition to the investigation of these prototype sensors, a specific fabrication batch with special passivation is also studied, allowing for a deeper understanding of the responsible mechanisms. This work presents an extensive study of this behaviour on large area sensors. The locations of the hotspots at the breakdown voltage at high humidity are revealed using different infrared thermography techniques. Several palliative treatments are attempted, proving the influence of sensor cleaning methods, as well as baking, on the device performance, but no improvement on the humidity sensitivity was achieved. Furthermore, a study of the incidence of the sensitivity in different batches is also presented, introducing a hypothesis of the origins of the humidity sensitivity associated to the sensor edge design, together with passivation thickness and conformity. Several actions to be taken during sensor production and assembly are extracted from this study, in order to minimize the impact of humidity sensitivity on the performance of large area silicon sensors for High Energy Physics experiments.
|
|
|
ATLAS Collaboration(Aad, G. et al), Amos, K. R., Aparisi Pozo, J. A., Bailey, A. J., Bouchhar, N., Cabrera Urban, S., et al. (2023). Measurement of the Sensitivity of Two-Particle Correlations in pp Collisions to the Presence of Hard Scatterings. Phys. Rev. Lett., 131(16), 162301–21pp.
Abstract: A key open question in the study of multiparticle production in high-energy pp collisions is the relationship between the “ridge”-i.e., the observed azimuthal correlations between particles in the underlying event that extend over all rapidities-and hard or semihard scattering processes. In particular, it is not known whether jets or their soft fragments are correlated with particles in the underlying event. To address this question, two-particle correlations are measured in pp collisions at collected by the ATLAS experiment at the LHC, with an integrated luminosity of 15.8 pb-1, in two different configurations. In the first case, charged particles associated with jets are excluded from the correlation analysis, while in the second case, correlations are measured between particles within jets and charged particles from the underlying event. Second-order flow coefficients, v2, are presented as a function of event multiplicity and transverse momentum. These measurements show that excluding particles associated with jets does not affect the measured correlations. Moreover, particles associated with jets do not exhibit any significant azimuthal correlations with the underlying event, ruling out hard processes contributing to the ridge. p= 13 TeV using data ffiffi s
|
|